国外阀门材料常用技术标准 镍合金锻件化学要求(2)_阀门标准

国外阀门材料常用技术标准 镍合金锻件化学要求(2)

成分,(%)
元素

镍-铁-铬

合金

UNS N08811

镍-铬-钼-铌

合金

UNS N06625

镍-铬-钼-钨

合金

UNS N06110

镍-铁-铬-

钼-铜合金

UNS N08825

低碳镍-钼-

铬合金

UNS N10276

低碳镍-钼-

铬合金

UNS N06022

铁-镍-铬-钼

-氮合金

UNS N08367

低碳镍-铬-

钼合金

UNS N06059

低碳镍-铬-

钼合金

UNS N06058

30.0-35.0 ≥58.0A ≥51.0A 38.0-46.0 残留元素A 残留元素A 23.50-25.50 平衡A 平衡
≤0.75 ≤0.50 1.5-3.0 ≤0.75 ≤0.50 ≤0.50
≥39.5A ≤5.0 ≤1.0 ≥22.0 4.0-7.0 2.0-6.0 残留元素A ≤1.5 ≤1.5
≤1.5 ≤0.5 ≤1.0 ≤1.0 ≤1.0 ≤0.50 ≤2.00 ≤0.5 ≤0.50
0.06-0.10 ≤0.10 ≤0.15 ≤0.05 ≤0.010 ≤0.015 ≤0.030 ≤0.010 ≤0.010
≤1.0 ≤0.5 ≤1.0 ≤0.5 ≤0.08 ≤0.08 ≤1.00 ≤0.10 ≤0.10
硫,≤ 0.015 0.015 0.015 0.03 0.03 0.02 0.030 0.010 0.010
19.0-23.0 20.0-23.0 28.0-33.0 19.5-23.5 14.5-16.5 20.0-22.5 20.0-22.0 22.0-24.0 20.0-23.0
0.15-0.60 ≤0.4 ≤1.0 ≤0.2 0.1-0.4 ≤0.40
0.15-0.60

≤0.4

≤1.0 0.6-1.2
铌+钽 3.15-4.15 ≤1.0
8.0-10.0 9.0-12.0 2.5-3.5 15.0-17.0 12.5-14.5 6.00-7.00 15.0-16.5 19.0-21.0
≤0.015 ≤0.50 ≤0.04 ≤0.02 ≤0.040 ≤0.015 ≤0.015
1.0-4.0 3.0-4.5 2.5-3.5 ≤0.3
≤2.5 ≤2.5 ≤0.3 ≤0.3
钒,≤ 0.35 0.35
0.18-0.25 0.02-0.15
铝+钛 0.85-1.20
镍+钼
铌,≤
锆,≤
文章来源:中国泵阀网